Structural performance of joints for partial reinforced beam using GFRP laminated plate and cylindrical reinforced LVL column

  • Song, Yojin
  • Jung, Hongju
  • Lee, Jung-jae
  • Suh, Jin-suk
  • Park, Sangbum
  • 외 1명
Citations

SCOPUS

2

초록

After being laminated with a combination of glass fiber reinforced plastic and plywood, the GFRP laminated plate was densificated for 1 hour at 150°C with pressure of 1.96 N/mm2. A partial reinforced beam was produced by attaching the 5 GFRP laminated plates to the joint of glulam and the column. In addition, the column to beam joint was produced by using reinforced laminated wooden pin which was made of GFRP sheet and plywood, fiber glass reinforced cylindrical-LVL column. The joint was made of round log, glulam and drift pin as the reference specimen, and its moment resistance was evaluated. As a result, the strength performance of specimens with partial reinforced beams were 1.8 times stronger than the reference specimen on average. Furthermore, rupture was neither occurred on partial reinforced beam nor column. Toughness and stiffness of joints were also fine. The GFRP sheet reinforced laminated plate showed better reinforcement effect than GFRP textile reinforced one. GFRP sheet was inserted into each layer of laminate, and it showed good condition in rotation-angle and strength, therefore it is the most appropriate to reinforce the part of the beam.

키워드

Cylindrical-LVLGFRP laminated plateGlass fiber reinforced plasticMoment resistanceReinforced laminated wooden pin
제목
Structural performance of joints for partial reinforced beam using GFRP laminated plate and cylindrical reinforced LVL column
저자
Song, YojinJung, HongjuLee, Jung-jaeSuh, Jin-sukPark, SangbumHong, Soonil
DOI
10.5658/WOOD.2014.42.3.282
발행일
2014
유형
Article
저널명
목재공학
42
3
페이지
282 ~ 289