Recovery of rare earth elements from coal fly ash using enrichment by sodium hydroxide leaching and dissolution by hydrochloric acid

Citations

WEB OF SCIENCE

26
Citations

SCOPUS

30

초록

The most common method to recover valuable rare earth elements from the potential resource coal fly ash is direct leaching in acidic solution. However, the extraction of rare earth elements using only acid leaching is not sufficiently effective due to the presence of Al-Si-based glasses. In the present work, pre-treatment using NaOH leaching was investigated to reduce the content of Al-Si-based phase before subjecting to acid leaching. The treatment at conditions NaOH 5 M, at 100 degrees C and for 120 min could dissolve 53% of the ash sample, and the rare earth contents were enriched from 267 mg/kg to 556 mg/kg. The NaOH leaching promote the further extraction of rare earth elements in all of acid medias (HCI, HNO3 and H2SO4), and HCI was the most effective leachant. More than 90% of rare earth elements was dissolved in 5 M HCI solution at 50 degrees C after 120 min. The combination of NaOH treatment and HCI leaching presented an effective approach to extract rare earth elements from coal fly ash with enrichment of rare earth element contents, increase the leaching efficiency and avoidance of harmful impacts to the environment due to the conventional pre-treatment using alkaline roasting.

키워드

Coal fly ash; rare earth elements; Al-Si-based phase; pre-treatment; NaOH leaching; acid leaching; EXTRACTION; COMBUSTION
제목
Recovery of rare earth elements from coal fly ash using enrichment by sodium hydroxide leaching and dissolution by hydrochloric acid
저자
Ha Bich Trinh; Kim, Seunghyun; Lee, Jaeryeong
DOI
10.1080/12269328.2022.2120092
발행일
2022-03-04
유형
Article
저널명
Geosystem Engineering
권
25
호
1-2
페이지
53 ~ 62