Shear strength of reinforced glulam-bolt connection by glass fiber combination

  • Kim, Keonho
  • Song, Yojin
  • Hong, Soonil
Citations

SCOPUS

4

초록

In order to know the shear performances of a bolted connection in reinforced glulam depending upon the combination of textile glass fiber, a tensile-type shear test was conducted. Textile glass fiber was used as a reinforcement, whose glass fiber arrangement was a plain weaving type or a diagonal cloth type. Reinforced glulam was made up of 5 plies and it was produced by inserting and laminating the plies between laminas depending upon a changed insert position and combination form of textile glass fiber. Tensile-type shear test specimens were a steel plate insert-type and joined at end-distance 7D with bolts whose diameter 12 or 16 mm. In textile glass fiber reinforced glulam, whose volume ratio was 1%, the yield shear strength of a 12 mm bolted connection increased by 10% when a test specimen had reinforced internal layers than when external layers were reinforced. As for textile glass fiber reinforced glulam, whose volume ratio was 2%, the yield shear strength of a 12 mm bolted connection increased significantly by about 22% compared to the bolted connection of non-reinforced glulam, and the yield shear strength of a 16 mm bolted connection was improved by about 20% compared to the bolted connection of non-reinforced glulam.

키워드

Bolt connectionGlass fiber reinforced glulamGlass fiber reinforced plasticShear performance
제목
Shear strength of reinforced glulam-bolt connection by glass fiber combination
저자
Kim, KeonhoSong, YojinHong, Soonil
DOI
10.5658/WOOD.2013.41.1.51
발행일
2013
유형
Article
저널명
목재공학
41
1
페이지
51 ~ 57