소각재와 커피슬러지를 이용한 건축외장재 제조

Preparation of Brick from MSWI Fly Ash and Coffee Sludge
  • 김태은
  • 정재아
  • 이우근

초록

With the advance of industrialization and urbanization, a lot of waste has been discharged and treated by incineration. In Korea, 441,004 ton of MSWI fly ash is discharged, which is composed of bottom ash (about 450,327 ton) and fly ash (about 92,755 ton) in 2008. MSWI fly ash generally contains high content of heavy metals, so it is regarded as hazardous waste. The objective of this research is to prepare brick made from waste materials such as MSWI fly ash, water sludge and coffee sludge. in this study. The optimum mixing ratio for these materials were 19.5% : 19.5% : 1% : 60%, respectively. They were dried at room temperature for 48 hrs, and heated for 4 hrs at 60℃ and for 6hrs at 100℃. After that, the dried bricks were sintered at 5℃/min to 1,115℃, and kept for 2 hrs at that temperature. Maximum compressive strength was 19.1 MPa at the optimal condition in our study.

키워드

MSWI fly ashCoffee sludgeBrickCompressive strengthKSLTMSWI fly ashCoffee sludgeBrickCompressive strengthKSLT
제목
소각재와 커피슬러지를 이용한 건축외장재 제조
제목 (타언어)
Preparation of Brick from MSWI Fly Ash and Coffee Sludge
저자
김태은정재아이우근
발행일
2010-12
유형
Y
저널명
한국폐기물자원순환학회지
27
8
페이지
687 ~ 693