상세 보기
초록
Feasibility of producing porous gradient structure by spark plasma sintering (SPS) process was examined. Adequate combination of porosity gradient and pore size distribution could be obtained by appropriately controlling the SPS parameter such as sintering temperature, sintering time, applied pressure, and stopper length. For the longitudinal porous gradient structure, pure W sample was prepared by specially shaped graphite mold. Stainless steel powder was employed for the radially layered porous structure with different pore size. The graded porous structure could be applied for the fabrication of W-Cu FGM by Cu-infiltration and high temperature filter with high filtration efficiency.
키워드
porosity gradient; pore size distribution; spark plasma sintering (SPS)
- 제목
- Fabrication of graded porous structure with pore size distribution by SPS process
- 저자
- Suk, Myung-Jin; Seo, Won-Sik; Kwon, Young-Soon
- 발행일
- 2007
- 유형
- Proceedings Paper
- 권
- 534-536
- 페이지
- 965 ~ +