In order to evaluate the bond performance of domestic larch glulam and the glass fiber reinforced plastic (GFRP) rod, the specimen with the GFRP rod bonded-in domestic larch glulam for pull-out test was produced. The test was carried out using various specimens with different gluing depth, width of glue-line and type of adhesive. The cantilever type rahmen structure specimen with bonded-in GFRP rods was produced based on the result of pull-out test, and its moment resistance performance was compared and examined with the moment resistance performance of slotted-in steel plate specimen. As a result of the pull-out test, the most excellent bond performance was found when the insertion depth of GFRP rods was 5 times larger than the diameter of GFRP rods. When the glue-line thickness was 1 mm, the bond performance improved by 17%∼29% in comparison to the bond performance in the case of the glue-line thickness of 2 mm. Also, the bonded strength of the specimen used with poly-urethane adhesive was 2.9∼4.0 times greater than the bonded strength of specimen used with resorcinol adhesive. The cantilever type rahmen structure specimen with bonded-in GFRP rods showed the moment resistance performance 0.82 times lower in comparison to the slotted-in steel plate specimen used with the drift pin, but the initial stiffness was similar as 0.93 times.
키워드
- 제목
- Moment resistance performance evaluation of larch glulam joint bonded in glass fiber reinforced plastic rods
- 저자
- Lee, In-hwan; Song, Yojin; Jung, Hongju; Hong, Soonil
- 발행일
- 2015
- 유형
- Article
- 저널명
- 목재공학
- 권
- 43
- 호
- 1
- 페이지
- 60 ~ 67