Mixed grinding with Na2S followed by water leaching was performed to extract Li from lepidolite. The leachability of Li increases dramatically in the ground mixture, regardless of the mixing ratio over the range of 1:1 to 3:1, while only 4.53% of Li was extracted in lepidolite ground without Na2S. The leachability increased with an increase of the grinding time, and ultimately, 93% of the Li was leached by water from the ground mixture with a weight ratio of 3:1 (Na2S:Lepidolite). In the process of the mixed grinding, the Li-contained lepidolite was destructured crystallographically, and it might have changed to different compounds. This process enables us to extract Li from lepidolite via a water leaching treatment.

키워드

lepidolitesodium sulfidemixed grindinglithiumwater leachingZINNWALDITE
제목
Extraction of Lithium from Lepidolite Using Mixed Grinding with Sodium Sulfide Followed by Water Leaching
저자
Lee, Jaeryeong
DOI
10.3390/min5040521
발행일
2015-12
유형
Article
저널명
Minerals
5
4
페이지
737 ~ 743