Pilling-Bedworth Ratio Approach to Surface Oxidation of Al-Mg Alloys Containing Al2Ca and Its Experimental Verification
- Ha, Seong-Ho;
- Yoon, Young-Ok;
- Kim, Bong-Hwan;
- Lim, Hyun-Kyu;
- Lee, Taeg-Woo;
- ... Lim, Sung-Hwan;
- 외 1명
Citations
WEB OF SCIENCE
17초록
Pilling-Bedworth ratio (PBR) of metal/dissimilar metal oxide and metal/mixed metal oxide for Al-Mg alloys containing Al2Ca was experimentally examined. The Al-7.5mass%Mg alloy exhibits a thick oxide layer due to the formation of MgO, primarily during the initial stage of oxidation at 788 K. As oxidation continues, the oxide layer of Al-7.5mass%Mg alloy develops an MgAl2O4-spineI. With the addition of 0.3mass%Al2Ca, the surface of the alloy exhibits a passivation effect. The alloy containing Al2Ca additive displays a combination of CaO, MgO and Al2O3 on its surface, and results in a PBR of similar to 1.
키워드
Al-Mg System; Pilling-Bedworth Ratio; Oxidation; Al2Ca
- 제목
- Pilling-Bedworth Ratio Approach to Surface Oxidation of Al-Mg Alloys Containing Al2Ca and Its Experimental Verification
- 저자
- Ha, Seong-Ho; Yoon, Young-Ok; Kim, Bong-Hwan; Lim, Hyun-Kyu; Lee, Taeg-Woo; Lim, Sung-Hwan; Kim, Shae K.
- 발행일
- 2018-05
- 유형
- Article
- 권
- 10
- 호
- 5
- 페이지
- 697 ~ 700
- 언어
- ENG
- 출판사
- AMER SCIENTIFIC PUBLISHERS
- 발행국가
- 미국
- 분량
- 4 페이지
- ISSN
- E 1947-2943
P 1947-2935