세라믹 촉매 담체의 내구 설계 기준에 대한 실험 및 수치해석의 비교

Comparison of Experimental and Numerical Analysis for Durability Design Criteria in Ceramic Catalyst Substrate

초록

This study examines thermal safety on three-way catalyst that dominates 70 % among whole exhaust gas purification device in 2003. Three-way catalyst durability in the Korea requires 5years/80,000 km in 1988 but require 10 years/120,000 km after 2002. Three-way catalyst durability in the USA requires 7 years/120,000 km but require 10 years/160,000 km after 2004. Three-way catalyst maintains high temperature in interior domain but maintains low temperature on outside surface. Therefore this device shows tensile stress on outside surface. Temperature distribution of three-way catalyst was acquired by thermal flow analysis for predicted thermal flow parameter. Thermal stress analysis for three-way catalysis was performed based on this temperature distribution. Thermal safety of three-way catalyst was estimated by power law dynamic fatigue life estimation and strength reduction methods for thermal stress.

키워드

Thermal Durability (열적 내구성)Dynamic Fatigue (동적 피로)Fluid-Structure Interaction (유동-구조 상호작용)Ceramic Catalyst Substrate (세라믹 촉매 담체)
제목
세라믹 촉매 담체의 내구 설계 기준에 대한 실험 및 수치해석의 비교
제목 (타언어)
Comparison of Experimental and Numerical Analysis for Durability Design Criteria in Ceramic Catalyst Substrate
저자
백석흠조석수
발행일
2010-09
유형
Y
저널명
한국정밀공학회지
27
9
페이지
58 ~ 66